摘 要
本文采用原位改性技术用环氧树脂来改性纳米SiO2,并将改性后的纳米SiO2和树脂混合液作为母料添加到纯环氧树脂中对其进行增韧。改性主要通过纳米SiO2表面的硅醇基(Si-OH)和环氧树脂的环氧基在一定条件下发生化学键接反应来实现。后期利用冲击测试、拉伸测试、傅里叶红外光谱仪(FTIR)、动态热机械分析(DMTA)等手段来对改性产物的性能和结构进行表征研究。实验中根据各项表征结果和力学性能测试数据来研究不同的改性条件对环氧树脂物理机械性能的具体影响。实验测试结果显示,改性纳米 SiO2的加入量1%为增韧环氧树脂的最佳比例,其冲击强度和拉伸模量存在最大值,分别增长了约37%和16.4%,而且玻璃化温度比纯环氧提高了23℃;当加入量为1.5%时,拉伸强度到达最大值44.38 MPa,增长5.6%,断裂伸长率也到达最大值,增长了3.5%。
关键词:环氧树脂 表面功能化 纳米SiO2 原位改性
Functional modification of Fumed silica with
Epoxy resin
Abstract
In this paper, the in-situ modification was performed with epoxy resin on the surface of fumed silica, then the mixture of modified nano-scaled silica and epoxy resin was added to the neat epoxy to toughen it. The modification was achieved by the chemical reaction of the silanol group of silica and the oxirane ring of epoxy compounds. The polymer structure and property were studied by means of Impact Test、Tensile Test 、FTIR and DMTA. We could study the different modification conditions on the physical and mechanical properties of epoxy resin compounds according to the results of the characterization and mechanical properties test data .
The results showed that when the additive amount of modified nano-scaled silica was 1%, the impact strength and tensile modulus reached maximum and increased by 37% and 16.4%,the glass transition temperature also reached the peak of 145℃ which was increased by 23℃; When the additive amount was 1.5%, the tensile strength reached the maximum value of 44.38 MPa, increased by 5.6%, the elongation at break also reached the maximum value, increased by 3.5%.
Key Words: Epoxy resin; Surface functionalization; Nano-silica; In-situ modification
目录
摘要............................................................................... .............Ⅰ
Abstract.......................................................................................Ⅱ
第一章 绪论............................................................................... . 1
1.1环氧树脂的定义及发展历程....................................1
1.2环氧树脂的结构特性及其应用概况..............................1
1.3环氧树脂的改性研究..........................................2
1.4纳米二氧化硅增韧环氧树脂的研究..............................3
1.5本实验内容简介及目的........................................4
第二章 实验部分....................................................................... . .6
2.1 实验仪器及设备.................................................................... 6
2.2 实验原料及药品.................................................................... 6
2.3 环氧树脂功能化改性纳米二氧化硅工艺流程................................. 7
2.4 环氧树脂功能化改性纳米二氧化硅实验...................................... 7
2.5 固化实验........................................................................... 10
2.6 力学性能测试实验................................................................10
2.7动态热机械分析(DMTA)测试................................................... 10
2.8傅里叶红外光谱仪(FTIR)测试............................................ .... 12
2.9热重分析(TG)测试........................................................... .... 12
第三章 结果与讨论............................................................... ......13
3.1 红外光谱分析......................................................................13
3.2 工艺条件对改性反应的影响....................................................14 3.3热重分析(TG)结果.................................................................16
3.4改性树脂动态机械热分析........................................................17
3.5 力学性能测试结果................................................................20
第四章 全文主要结论............................................................... ...23
4.1 主要结论......................................................................... ..23
4.2 研究工作不足及展望........................................................... .23
参考文献.................................................................................. . .24
致谢.................................................................................. . .... ...26
第一章 绪 论
1.1 环氧树脂的定义及发展历程
1.1.1 定义
环氧树脂(Epoxy Resin)是指有2个或以上数量的环氧基,主体结构为脂肪族或芳香族等有机化合物并且能通过分子结构中环氧基团的化学反应形成热固性材料的高分子低聚体(Oligomer)[12]。
1.1.2 发展历程
相关图片展示:
您可能感兴趣的文章
- 可聚合高分子模板增强制备高耐久超疏水涂层文献综述
- PVC/ABS合金的制备及性能研究开题报告
- 设计具有增强的赝电容及电催化性能的Co3O4/NiCo2O4双壳纳米笼结构外文翻译资料
- 光子上转换手性液晶:显著放大的上转换圆偏振发光外文翻译资料
- 氧空位型LiV3O8纳米片的快速稳定储锂性能研究外文翻译资料
- 应用于高性能钙钛矿太阳能电池的电子传输层的前体工程外文翻译资料
- 复合材料科学与技术 ——含碳纳米管的多孔导电弹性体复合材料悬浮在共连续聚合物的狭窄孔隙中的混合纳米复合材料外文翻译资料
- 一种用于先进锂硫电池源自聚罗丹宁纤维素的氮硫双掺杂碳外文翻译资料
- 短玻璃纤维增强聚丙烯控制界面和力学性能参数外文翻译资料
- 含Ca0的LaCO.0H纳米齿轮及其发光和脱NOx性能外文翻译资料